Grade


AMS

Other Specifications

Description

Ni

Fe

Cr

Cu
Density
(lb./ cu.in.)
Nickel 200
N02200
  ASTM B-160
ASTM B-162
Commercially pure nickel. High corrosion resistance. Electrodes, electronics, food processing. 99.5 .20   .13 .321
Nickel "400"
N04400
4544
4675
ASTM B-127
ASTM B-164
High strength, good weld-ability, excellent corrosion resistance over wide range of temperatures 66.5 1.25   31.5 .319
Nickel "K-500"
N05500
4676 QQ-N-286 Age hardenable version of Alloy 400 for increased strength and hardness. 66.5 1.0   29.5 .306
Alloy 600
N06600
5540
5665
ASTM B-168
ASTM B-163
High nickel, high chromium content for oxidation resistance in corrosive environments at elevated temps. 76.0 8.0 15.5 .25 .304
Alloy 625
N06625
5599
5666
ASTM B-443
ASTM B-446
High strength and toughness from cryogenic temperatures to 1800°F. Good oxidation resistance. 61.0 2.5 21.5   .305
Alloy 718
N07718
5596
5662
ASTM B-637
ASTM B-670
Excellent strength from 423°F to 1300°F. Age hardenable w/excellent oxidation resistance up to 1800°F. 52.5 18.5 19.0 .15 .296
Alloy X-750
N07750
5598
5667
ASTM B-637 Age hardenable alloy w/good corrosion and oxidation resistance. 73.0 7.0 15.5 .25 .296
Alloy C-276
N10276
5530
5750
ASTM B-574
ASTM B-575
Excellent resistance to pitting and stress corrosion cracking. Good fabricability. 55.0 6.0 16.0   .321
Alloy "X"
N06002
5536
5754
ASTM B-435 Excellent strength and oxidation resistance to 2200°F. 48.0 18.5 21.8   .297